Abstract

Primary dendrite spacings and side-branch coarsening kinetics were examined in specimens of the single-crystal multicomponent commercial superalloy PWA - 1480 , which were directionally solidified in a positive thermal gradient. The experimentally observed dependence of primary dendrite spacings and side-branch coarsening kinetics on growth rate and thermal gradient were in agreement with the behavior predicted by analytical models developed for binary alloys.